JPS5117937A
JPS5117937AJP50065205AJP6520575AJPS5117937AJP S5117937 AJPS5117937 AJP S5117937AJP 50065205 AJP50065205 AJP 50065205AJP 6520575 AJP6520575 AJP 6520575AJP S5117937 AJPS5117937 AJP S5117937A
Authority
JP
Japan
Prior art keywords
mixture
propylene
weight
parts
ethylene
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
JP50065205A
Other languages
Japanese (ja)
Other versions
JPS5920693B2 (en
Inventor
Myuure Anjero
Amadei Otsutabio
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
ExxonMobil Technology and Engineering Co
Original Assignee
Exxon Research and Engineering Co
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Exxon Research and Engineering CofiledCriticalExxon Research and Engineering Co
Publication of JPS5117937ApublicationCriticalpatent/JPS5117937A/ja
Publication of JPS5920693B2publicationCriticalpatent/JPS5920693B2/en
Expiredlegal-statusCriticalCurrent

Links

Classifications

Landscapes

Abstract

A mixture containing a homogeneous mixture of a propylene-ethylene copolymer containing from 20 to 35 mol% of ethylene and at least 30 parts by weight of finely divided conductive carbon per 100 parts by weight of copolymer can be prepared by mixing at a high shear rate, for example in a Banbury mixer, at a propylene-ethylene copolymer temperature of at least 100 DEG C. A mixture of this type is suitable for the production of a two-pole plate for an electrochemical cell.
JP50065205A1974-06-041975-05-30 Conductive polyolefin compositionExpiredJPS5920693B2 (en)

Applications Claiming Priority (2)

Application NumberPriority DateFiling DateTitle
GB24665741974-06-04
GB24665/74AGB1495275A (en)1974-06-041974-06-04Conductive polyolefin compositions

Publications (2)

Publication NumberPublication Date
JPS5117937Atrue JPS5117937A (en)1976-02-13
JPS5920693B2 JPS5920693B2 (en)1984-05-15

Family

ID=10215319

Family Applications (1)

Application NumberTitlePriority DateFiling Date
JP50065205AExpiredJPS5920693B2 (en)1974-06-041975-05-30 Conductive polyolefin composition

Country Status (12)

CountryLink
JP (1)JPS5920693B2 (en)
BE (1)BE829684A (en)
BR (1)BR7503341A (en)
CA (1)CA1057948A (en)
CH (1)CH618453A5 (en)
DE (1)DE2524640C2 (en)
FR (1)FR2273843A1 (en)
GB (1)GB1495275A (en)
IT (1)IT1038259B (en)
NL (1)NL181875C (en)
SE (1)SE411355B (en)
ZA (1)ZA753080B (en)

Cited By (4)

* Cited by examiner, † Cited by third party
Publication numberPriority datePublication dateAssigneeTitle
JPS53165813U (en)*1977-06-021978-12-26
JPS61161664A (en)*1985-01-091986-07-22Mitsubishi Pencil Co LtdManufacture of separator for fuel cell
JPS6282653A (en)*1985-10-041987-04-16Fuji Electric Co Ltd Method for manufacturing fuel cell separate plates
US4971726A (en)*1987-07-021990-11-20Lion CorporationElectroconductive resin composition

Families Citing this family (11)

* Cited by examiner, † Cited by third party
Publication numberPriority datePublication dateAssigneeTitle
JPS5716041A (en)*1980-05-231982-01-27Kureha Chem Ind Co LtdElectrically conductive molding resin composite material
DE3034747C2 (en)*1980-09-151985-01-17kabelmetal electro GmbH, 3000 Hannover Process for the production of a polymer mixture containing carbon black and its use for electrical cables
DE3382280D1 (en)*1982-11-171991-06-13Meidensha Electric Mfg Co Ltd ELECTRICALLY CONDUCTIVE PLASTIC.
US4610811A (en)*1984-03-071986-09-09Mitsui Toatsu Chemicals, Inc.Iodine-containing conductive resin composition
JPS6158850A (en)*1984-08-311986-03-26株式会社村田製作所Carbonaceous formed body
FR2574803B1 (en)*1984-12-181987-01-30Occidental Chem Co ELECTRICALLY CONDUCTIVE THERMOPLASTIC MATERIAL AND METHOD FOR MANUFACTURING SUCH MATERIAL
DE3824139A1 (en)*1988-07-151990-01-25Siemens Ag ELECTRODES FOR PIEZOCERAMICS
KR100417050B1 (en)*1999-10-212004-02-05마쯔시다덴기산교 가부시키가이샤Polymer electrolyte fuel cell
NL1014403C1 (en)*2000-02-172001-08-20Nedstack Holding B V Method for manufacturing a plate-shaped semi-finished product that is suitable for use in, among others, Polymer Electrolyte Fuel Cells.
JP2002298865A (en)*2001-03-302002-10-11Nichias Corp Fuel cell separator and method of manufacturing the same
JP4388278B2 (en)*2001-05-112009-12-24株式会社クレハ Separator for polymer electrolyte fuel cell and method for producing the same

Family Cites Families (2)

* Cited by examiner, † Cited by third party
Publication numberPriority datePublication dateAssigneeTitle
US3591526A (en)*1968-01-251971-07-06Polyelectric CorpMethod of manufacturing a temperature sensitive,electrical resistor material
DE2118135C3 (en)*1971-04-141980-01-24Kabel- Und Metallwerke Gutehoffnungshuette Ag, 3000 Hannover Conductive polymer mixture

Cited By (4)

* Cited by examiner, † Cited by third party
Publication numberPriority datePublication dateAssigneeTitle
JPS53165813U (en)*1977-06-021978-12-26
JPS61161664A (en)*1985-01-091986-07-22Mitsubishi Pencil Co LtdManufacture of separator for fuel cell
JPS6282653A (en)*1985-10-041987-04-16Fuji Electric Co Ltd Method for manufacturing fuel cell separate plates
US4971726A (en)*1987-07-021990-11-20Lion CorporationElectroconductive resin composition

Also Published As

Publication numberPublication date
GB1495275A (en)1977-12-14
SE411355B (en)1979-12-17
SE7506230L (en)1975-12-05
NL181875B (en)1987-06-16
FR2273843A1 (en)1976-01-02
JPS5920693B2 (en)1984-05-15
BE829684A (en)1975-12-01
DE2524640C2 (en)1983-07-28
NL181875C (en)1987-11-16
FR2273843B1 (en)1981-08-28
DE2524640A1 (en)1975-12-18
CH618453A5 (en)1980-07-31
CA1057948A (en)1979-07-10
ZA753080B (en)1976-04-28
IT1038259B (en)1979-11-20
BR7503341A (en)1976-05-25
NL7506613A (en)1975-12-08

Similar Documents

PublicationPublication DateTitle
FR2273843B1 (en)
GB1512364A (en)Substituted lithium orthosilicates and solid electrolytes therefrom
JPS5549862A (en)Nonaqueous electrolytic battery
GB1507691A (en)Process for the preparation of pulverulent batches of rubber and filler
ES439662A1 (en)Method of producing biologically active compositions
ES486851A1 (en)Process for the production of ursodesoxycholic acid
ES441583A1 (en)Process for the continuous polymerisation of lactams
JPS57187878A (en)Nonaqueous electrolyte solution for secondary lithium battery
GB1443134A (en)Fluorinated carbon compositions
GB530859A (en)Improvements in or relating to galvanic dry cells
JPS573368A (en)Preparation of positive active material for nonaqueous battery
GB622512A (en)Improvements relating to electric accumulators
JPS6482456A (en)Manufacture of positive electrode for nonaqueous electrolyte cell
JPS5546269A (en)Dry cell
JPS57121157A (en)Electrode of metal-bromine battery
JPS544296A (en)Production of carbon electrode
JPS57174863A (en)Organic electrolyte cell
JPS5765675A (en)Electrolyte matrix for fuel cell and its manufacture
JPS5636865A (en)Manufacture of active material for plate of lead storage battery
JPS57141875A (en)Solid electrolyte battery
JPS57145273A (en)Solid electrolyte battery
JPS5546268A (en)Dry cell
JPS55122359A (en)Cell
NICHOLSONNew cathode material for high energy density batteries(considering semiconductive metal fluorides)[Final Report, 1 Sep. 1972- 30 Jun. 1973]
JPS56120072A (en)Solid electrolyte battery