| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| GB948468AGB1253681A (en) | 1968-02-27 | 1968-02-27 | Improvements in or relating to the toughening of glass |
| IE22669AIE33410B1 (en) | 1968-02-27 | 1969-02-20 | Improvements in or relating to the toughening of glass |
| DE19691910086DE1910086C3 (en) | 1968-02-27 | 1969-02-25 | Method and device for hardening a pane of soda-lime-silicate glass |
| SE256469ASE348451B (en) | 1968-02-27 | 1969-02-25 | |
| SE939272ASE366286B (en) | 1968-02-27 | 1969-02-25 | |
| DK106369ADK137747B (en) | 1968-02-27 | 1969-02-26 | Method for curing a sheet of soda-lime-silica glass and apparatus for carrying out the method. |
| FR6904881AFR2002674A1 (en) | 1968-02-27 | 1969-02-26 | |
| PL13199869APL69829B1 (en) | 1968-02-27 | 1969-02-27 | |
| CS142369ACS166692B2 (en) | 1968-02-27 | 1969-02-27 | |
| AT200769AAT316785B (en) | 1968-02-27 | 1969-02-27 | Method and device for hardening a glass plate |
| NL6903047ANL6903047A (en) | 1968-02-27 | 1969-02-27 | |
| ZM3469AZM3469A1 (en) | 1968-02-27 | 1969-02-27 | Improvements in or relating to the toughening of glass |
| BE729055DBE729055A (en) | 1968-02-27 | 1969-02-27 | |
| BR20672069ABR6906720D0 (en) | 1968-02-27 | 1969-02-27 | PERFECT PROCESS AND APPLIANCE FOR GLASS ENRICHMENT AND ITS PRODUCT |
| CH295469ACH527776A (en) | 1968-02-27 | 1969-02-27 | Process for tempering glass, glass tempered by the process and device for carrying out the process |
| US155234AUS3890128A (en) | 1968-02-27 | 1971-06-21 | Method of toughening glass |
| NO39372ANO128566B (en) | 1968-02-27 | 1972-02-11 |
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| GB948468AGB1253681A (en) | 1968-02-27 | 1968-02-27 | Improvements in or relating to the toughening of glass |
| Publication Number | Publication Date |
|---|---|
| GB1253681Atrue GB1253681A (en) | 1971-11-17 |
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| GB948468AExpiredGB1253681A (en) | 1968-02-27 | 1968-02-27 | Improvements in or relating to the toughening of glass |
| Country | Link |
|---|---|
| AT (1) | AT316785B (en) |
| BE (1) | BE729055A (en) |
| BR (1) | BR6906720D0 (en) |
| CH (1) | CH527776A (en) |
| CS (1) | CS166692B2 (en) |
| DE (1) | DE1910086C3 (en) |
| DK (1) | DK137747B (en) |
| FR (1) | FR2002674A1 (en) |
| GB (1) | GB1253681A (en) |
| IE (1) | IE33410B1 (en) |
| NL (1) | NL6903047A (en) |
| PL (1) | PL69829B1 (en) |
| SE (2) | SE348451B (en) |
| ZM (1) | ZM3469A1 (en) |
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| DE2434616A1 (en)* | 1973-07-20 | 1975-01-30 | Triplex Safety Glass Co | METHOD OF HARDENING GLASS |
| US9296638B2 (en) | 2014-07-31 | 2016-03-29 | Corning Incorporated | Thermally tempered glass and methods and apparatuses for thermal tempering of glass |
| CN112624585A (en)* | 2020-12-07 | 2021-04-09 | 宁波大学 | Method for manufacturing physical toughened glass cylindrical rod |
| CN113528787A (en)* | 2021-07-20 | 2021-10-22 | 南京劲拓机械有限公司 | Improve heat treatment system of carburization part quenching hardness HRC58 platform |
| US11485673B2 (en) | 2017-08-24 | 2022-11-01 | Corning Incorporated | Glasses with improved tempering capabilities |
| CN115521052A (en)* | 2022-10-12 | 2022-12-27 | 索奥斯(广东)玻璃技术股份有限公司 | Glass tempering production line using double-chamber heating furnace |
| US11643355B2 (en) | 2016-01-12 | 2023-05-09 | Corning Incorporated | Thin thermally and chemically strengthened glass-based articles |
| US11697617B2 (en) | 2019-08-06 | 2023-07-11 | Corning Incorporated | Glass laminate with buried stress spikes to arrest cracks and methods of making the same |
| US11708296B2 (en) | 2017-11-30 | 2023-07-25 | Corning Incorporated | Non-iox glasses with high coefficient of thermal expansion and preferential fracture behavior for thermal tempering |
| US11795102B2 (en) | 2016-01-26 | 2023-10-24 | Corning Incorporated | Non-contact coated glass and related coating system and method |
| US11891324B2 (en) | 2014-07-31 | 2024-02-06 | Corning Incorporated | Thermally strengthened consumer electronic glass and related systems and methods |
| US12064938B2 (en) | 2019-04-23 | 2024-08-20 | Corning Incorporated | Glass laminates having determined stress profiles and methods of making the same |
| US12338159B2 (en) | 2015-07-30 | 2025-06-24 | Corning Incorporated | Thermally strengthened consumer electronic glass and related systems and methods |
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| DE3001944C2 (en)* | 1980-01-21 | 1982-04-29 | Schott Glaswerke, 6500 Mainz | Process for the thermal toughening of glass |
| US4445921A (en)* | 1983-01-24 | 1984-05-01 | Ppg Industries, Inc. | Tempering glass sheets by cooling comprising sublimation quenching |
| US8234883B2 (en) | 2005-11-29 | 2012-08-07 | Ppg Industries Ohio, Inc. | Apparatus and method for tempering glass sheets |
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| NL48420C (en)* | 1936-11-05 | |||
| BE425382A (en)* | 1936-12-22 | |||
| US2365967A (en)* | 1939-06-22 | 1944-12-26 | American Securit Co | Method of tempering glass |
| US3169900A (en)* | 1955-01-31 | 1965-02-16 | Libbey Owens Ford Glass Co | Stress pattern tempered glass sheet and method of making the same |
| LU36540A1 (en)* | 1957-10-30 |
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| DE2434616A1 (en)* | 1973-07-20 | 1975-01-30 | Triplex Safety Glass Co | METHOD OF HARDENING GLASS |
| US11891324B2 (en) | 2014-07-31 | 2024-02-06 | Corning Incorporated | Thermally strengthened consumer electronic glass and related systems and methods |
| US10233111B2 (en) | 2014-07-31 | 2019-03-19 | Corning Incorporated | Thermally tempered glass and methods and apparatuses for thermal tempering of glass |
| US9783448B2 (en) | 2014-07-31 | 2017-10-10 | Corning Incorporated | Thin dicing glass article |
| US9802853B2 (en) | 2014-07-31 | 2017-10-31 | Corning Incorporated | Fictive temperature in damage-resistant glass having improved mechanical characteristics |
| US9975801B2 (en) | 2014-07-31 | 2018-05-22 | Corning Incorporated | High strength glass having improved mechanical characteristics |
| US10005691B2 (en) | 2014-07-31 | 2018-06-26 | Corning Incorporated | Damage resistant glass article |
| US10077204B2 (en) | 2014-07-31 | 2018-09-18 | Corning Incorporated | Thin safety glass having improved mechanical characteristics |
| US9296638B2 (en) | 2014-07-31 | 2016-03-29 | Corning Incorporated | Thermally tempered glass and methods and apparatuses for thermal tempering of glass |
| US9776905B2 (en) | 2014-07-31 | 2017-10-03 | Corning Incorporated | Highly strengthened glass article |
| US12338159B2 (en) | 2015-07-30 | 2025-06-24 | Corning Incorporated | Thermally strengthened consumer electronic glass and related systems and methods |
| US11643355B2 (en) | 2016-01-12 | 2023-05-09 | Corning Incorporated | Thin thermally and chemically strengthened glass-based articles |
| US11795102B2 (en) | 2016-01-26 | 2023-10-24 | Corning Incorporated | Non-contact coated glass and related coating system and method |
| US11485673B2 (en) | 2017-08-24 | 2022-11-01 | Corning Incorporated | Glasses with improved tempering capabilities |
| US11708296B2 (en) | 2017-11-30 | 2023-07-25 | Corning Incorporated | Non-iox glasses with high coefficient of thermal expansion and preferential fracture behavior for thermal tempering |
| US12410090B2 (en) | 2017-11-30 | 2025-09-09 | Corning Incorporated | Non-iox glasses with high coefficient of thermal expansion and preferential fracture behavior for thermal tempering |
| US12064938B2 (en) | 2019-04-23 | 2024-08-20 | Corning Incorporated | Glass laminates having determined stress profiles and methods of making the same |
| US11697617B2 (en) | 2019-08-06 | 2023-07-11 | Corning Incorporated | Glass laminate with buried stress spikes to arrest cracks and methods of making the same |
| US12043575B2 (en) | 2019-08-06 | 2024-07-23 | Corning Incorporated | Glass laminate with buried stress spikes to arrest cracks and methods of making the same |
| CN112624585A (en)* | 2020-12-07 | 2021-04-09 | 宁波大学 | Method for manufacturing physical toughened glass cylindrical rod |
| CN113528787A (en)* | 2021-07-20 | 2021-10-22 | 南京劲拓机械有限公司 | Improve heat treatment system of carburization part quenching hardness HRC58 platform |
| CN113528787B (en)* | 2021-07-20 | 2022-08-09 | 南京劲拓机械有限公司 | Improve heat treatment system of carburization part quenching hardness HRC58 platform |
| CN115521052B (en)* | 2022-10-12 | 2024-03-19 | 索奥斯(广东)玻璃技术股份有限公司 | Glass tempering production line using double-chamber heating furnace |
| CN115521052A (en)* | 2022-10-12 | 2022-12-27 | 索奥斯(广东)玻璃技术股份有限公司 | Glass tempering production line using double-chamber heating furnace |
| Publication number | Publication date |
|---|---|
| CH527776A (en) | 1972-09-15 |
| IE33410L (en) | 1969-08-27 |
| ZM3469A1 (en) | 1970-10-19 |
| CS166692B2 (en) | 1976-03-29 |
| SE366286B (en) | 1974-04-22 |
| DE1910086C3 (en) | 1975-07-17 |
| NL6903047A (en) | 1969-08-29 |
| FR2002674A1 (en) | 1969-10-31 |
| DK137747C (en) | 1978-10-09 |
| DK137747B (en) | 1978-05-01 |
| BR6906720D0 (en) | 1973-01-25 |
| AT316785B (en) | 1974-07-25 |
| DE1910086A1 (en) | 1969-10-02 |
| BE729055A (en) | 1969-08-27 |
| DE1910086B2 (en) | 1974-11-28 |
| IE33410B1 (en) | 1974-06-26 |
| SE348451B (en) | 1972-09-04 |
| PL69829B1 (en) | 1973-10-31 |
| Publication | Publication Date | Title |
|---|---|---|
| GB1253681A (en) | Improvements in or relating to the toughening of glass | |
| US3223501A (en) | Method and apparatus for treating glass on a pressurized fluid bed | |
| TW376378B (en) | Method and apparatus of bending and tempering a thin glass sheet | |
| GB769692A (en) | Improvements in or relating to the manufacture of flat glass | |
| GB1220292A (en) | Process for tempering vitreous and vitro-crystalline bodies | |
| GB1383201A (en) | Glass ceramic material | |
| ES438603A1 (en) | Method of and apparatus for bending and tempering thin glass sheets | |
| ES361622A1 (en) | Tempered stemware and process of making it | |
| US3251671A (en) | Method of annealing of glass ribbon | |
| GB1298899A (en) | Process for producing tempered glass sheet | |
| GB1405663A (en) | Cutting glass | |
| US3245772A (en) | Method of heat treating glass sheets while being conveyed | |
| GB1289488A (en) | ||
| US3293021A (en) | Method of heating glass sheets | |
| GB1133615A (en) | Improvements in or relating to methods of toughening glass in sheet form | |
| US3251670A (en) | Differential thermal treatment of glass objects | |
| GB797101A (en) | Improvements relating to the manufacture of flat glass in continuous ribbon form | |
| US3298810A (en) | Method and apparatus for bending and tempering glass sheets | |
| NZ220787A (en) | Heat strengthening of glass: intermittent discontinuous support for glass during cooling | |
| GB1208153A (en) | Glass tempering processes and apparatus | |
| GB1160284A (en) | Tempering | |
| ES365286A1 (en) | Method for vertical suspension of glass sheets during thermal treatment | |
| US3374077A (en) | Method of press bending glass sheets between cold opposed shaping molds | |
| ES298701A1 (en) | Methods of heat treating and gas pressure supporting glass in sheet form | |
| GB1034077A (en) | Improvements in or relating to apparatus and a method for annealing glass |